Cryoarc 316L-15


Cryoarc 316L-15 electrodes are designed to be used in cryogenic applications where impact toughness is required. Cryoarc electrodes can also be used where low magnetic permeability is required.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength
As Welded 45 % 80 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 35 ft-lb -320 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCSiFerrite FNNiNCr
2.0 %2.2 %0.03 %0.5 %5 %13.6 %0.05 %18.0 %

Classifications: SFA/AWS A5.4; 316L-15

Alloy Type: Austenitic CrNiMo
Coating Type: Basic
Ferrite Content: max. FN 2