OK Autrod 16.38


A continuous solid corrosion resisting non-magnetic chromium-nickel-molybdenium wire for welding of stabilized and non-stabilized austenitic alloys of the same type as well as non magnetic steels. OK Autrod 16.38 can be used in combination with OK Flux 10.93 The alloy is corrosion resistant in seawater environment at temperatures below 350°C and has very good corrosion resistance to acids such as nitric acid. Excellent impact properties at low temperatures.

Where To Buy


Specifications


Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCSiNiNCr
6.9 %3.0 %0.01 %0.4 %16.5 %0.18 %19.9 %

Classifications: EN ISO 14343-A; S 20 16 3 Mn L; Wire Electrode

Alloy Type: Austenitic (7 % Mn - 20 % Cr - 16 % Ni - 3 % Mo)