Weld 6013

Weld 6013

Sureweld 6013 is an all-position electrode. The arc is very stable even when low-voltage open circuit transformers are used. The power of its arc allows depositing quick welds, medium penetration, and good appearance. Sureweld 6013 eliminates the risk of trapping the slag due to its special characteristics and mineral coating. Sureweld 6013 is used on a wide array of mild steel fabrication where ease of operation and good appearance is required. Sureweld 6013 is recommended for welding vehicle bodies, profiles, tanks, ducts chassis, freight cars, ornamental jobs and thin-sheet structures.

Where To Buy


Industries

  • Industrial and General Fabrication
  • Mobile Equipment
  • Ship/Barge Building

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 27 % 55 % 81 ksi 70 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 35 ft-lb 32 °F

Approvals: CWB CSA W48, E4913
Classifications: AWS A5.1, E6013

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Carbon Manganese
Coating Type: IMPERIAL_Rutile-acid covering
Welding Current: AC, DC+