SUREWELD 7014

SUREWELD 7014

Sureweld 7014 is an iron powder coated electrode permitting the use of higher welding currents while improving the deposition rate. The use of an iron-powder coating also improves deposition efficiency. High speeds and high heats can be used without undercut. Slag removal is excellent. Sureweld 7014 is widely used for welding mild steels such as ASTM A-36, A-113, A-283, A-284, A-285, A-306, A-515 and A-516. Typical applications include construction equipment, metal fixtures, automotive parts, barges and farm machinery.

Where To Buy


Industries

  • Industrial and General Fabrication
  • Mobile Equipment
  • Ship/Barge Building

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 28 % 64 % 71 ksi 61 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnCSSi
0.02 %0.30 %0.04 %0.02 %0.14 %

Classifications: AWS A5.1; E7014