All-State 88-T

All-State 88-T

How to order


Specifications


Typical Tensile Properties

Elongation Reduction in Area Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength Condition
29 % 58 % 1150 °F 8 hr 80 ksi 64 ksi -
26 % 58 % - - 86 ksi 68 ksi As Welded

View full specs

A mild steel, copper coated TIG rod with good wetting characteristics, and excellent bead appearance. Can be used on uncleaned metal.