All-State 275 SUPER

An AC/DC reverse, all-position electrode producing an outstanding bead appearance. Use on tool,high alloy, aircraft, spring, nickel-clad, stainless, and dissimilar steels. Excellent for dirty, greasy, and rusty metals. Machinable.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 22-25 % up to 120 ksi 94 ksi