All-State 252

This AC/DC reverse, all-position electrode is used for welding 310 and 314 stainless subjected to corrosion and elevated temperatures, as well as dissimilar steels and stainless of unknown analysis.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Hardness (HRC) Tensile Strength Yield Strength
As Welded 35-45 % B85-B85 HRC 95 ksi 65 ksi