All-State GLIDEARC

All-State GLIDEARC

Special vertical up, vertical down, and overhead stainless steel for maintenance applications. It is ideal for poor fit-up joints in all positions.

Add to shopping list


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 42 % up to 80 ksi up to 56 ksi