All-State ALL-SHIELD 316L

All-State ALL-SHIELD 316L

How to order


Specifications


Typical Tensile Properties

75% Ar / 25% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 36 % 89 ksi 69 ksi

View full specs

All-position, DC reverse, flux cored stainless steel wire with self-peeling slag. Excellent for welding type 316 stainless. Resists corrosion from sulphuric and sulphurous acids, cellulose solutions, and chlorides. For best results, use with a 75% Argon/25% CO2 shielding gas. Meets AWS A5.22,Class E316LT-1.

Add to shopping list


Specifications


Typical Tensile Properties

75% Ar / 25% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 36 % 89 ksi 69 ksi