All-State ALL-SHIELD 308L

All-State ALL-SHIELD 308L

How to order


Specifications


Typical Tensile Properties

75% Ar / 25% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 45 % 86 ksi 58 ksi

View full specs

All-position, DC reverse, flux cored stainless steel wire with self-peeling slag. Excellent for welding stainless types 301, 302, 304, 304L, 308 and 308L. Also for use on types 321 and 347, provided the service temperature does not exceed 500°F (260°C) For best results, use with a 75%Argon/25% CO2 shielding gas. Meets AWS A5.22, Class E38LT-1.

Add to shopping list


Specifications


Typical Tensile Properties

75% Ar / 25% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 45 % 86 ksi 58 ksi