All-State 309L

All-State 309L

How to order


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength
As Welded 35-45 % up to 90 ksi

View full specs

All-State® 309L is an electrode with excellent starting properties on all types of AC welding|equipment. The arc is stable, smooth, with fine spray weld metal transfer. The bead is uniform,|flat or slightly concave with straight-line feathered edges. Penetration is complete and the weld|metal is free from porosity. Slag is easily and completely removed without secondary film which|means less cleaning, grinding and polishing time. This electrode has good out-of-position|characteristics.|All-State® 309L is used primarily in the overlay of steel where inter-granular corrosion must be|kept to a minimum and for welding mild or carbon steel to stainless steel provided the service|temperature is less than 600°F (316°C). Carbon content 0.04% maximum.

Add to shopping list


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength
As Welded 35-45 % up to 90 ksi

x

Inquire about the All-State 309L



×

Find the Closest Distributor

x

Find the Closest Distributor

x

x

Loading..