All-State 308L HI-SIL

All-State 308L HI-SIL

How to order


Specifications


Classifications: AWS A5.9

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 42 % up to 86 ksi 62 ksi

View full specs

A smooth drawn, uniform surfaced stainless steel wire useful in applications where uniform appearance is essential. For use on stainless steel types 304, 305, 308, 308L, 321 and 347 as well as other 18-9 stainless steels where carbide precipitation may arise.