ESAB

All-State 430 Sldr

All-State 430 Sldr

Cadmium free, low temperature, food grade, solder for high strength on stainless steels, and dissimilar metals. Deposits closely match stainless, and stay bright after prolonged service. Use with All-State Duzall flux or All-state 430 flux.

Where To Buy


Specifications


Typical Tensile Properties

Condition Tensile Strength
As Welded 15 ksi