Previous Next

ESAB

All-State 101FC CAD FR

45% flux coated silver brazing alloy for use on light gauge material and tight fitting joints. Excellent capillary flow on ferrous and non-ferrous metals or combinations of both (excluding white metals) Excellent for food processing or food handling equipment. Use with All-State No. 110 or All-State S-200 flux.