Bare corrosion and heat-resisting Ni-Cr-Mo rods for welding of high alloyed heat-resisting and corrosion resisting materials, 9%Ni-steels and similar steels with high notch toughness at low temperatures. Also for joining of dissimilar metals of the types mentioned. The weld metal has very good mechanical properties at high and low temperatures. Good resistance to pitting and stress corrosion.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
40 % 113 ksi 80 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
74 ft-lb -321 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCSiNiNb+TaCrFe
0.04 %8.6 %0.02 %0.06 %64.8 %3.5 %22.7 %0.3 %

Approvals: DNV; For NV1.5Ni up to NV9Ni; VdTÜV; 12460
Classifications: SFA/AWS A5.14; ERNiCrMo-3; Wire Electrode; EN ISO 18274; S Ni 6625; Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Alloyed nickel (Ni + 22 % Cr + 9 % Mo - 3.5 % Nb)