OK Tigrod NiCrMo-13


Bare Ni-Cr-Mo rods for welding of high alloyed Ni-base materials, 9% Ni steel and super austenic steels of type 20Cr-25Ni with 4-6% Mo. Can also be used for welding carbon steel to Ni base steel. The weld metal has a very good toughness and is corrosion resistant over a wide range of applications in oxidizing and reducing media.

Add to shopping list


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
40 % 109 ksi 72.5 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
88.5 ft-lb -166 °F

Typical Weld Metal Analysis %

MnMoCSiNiAlCrFe
0.2 %16.0 %0.01 %0.1 %61.0 %0.3 %23.0 %1.0 %

Approvals: VdTÜV, 12663 (MV)
Classifications: SFA/AWS A5.14, ERNiCrMo-13, Wire Electrode, EN ISO 18274, S Ni 6059 (NiCr23Mo16), Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Alloyed nickel (Ni + 23 % Cr + 16 % Mo)