OK Tigrod Ni-1


A bare nickel based rod alloyed with about 3% Ti for welding of high purity nickel (min 99.6 %Ni), ordinary wrought nickel and nickel with reduced C content. The weld metal can be used in a wide range of applications were the construction is working with corrosive media.

Where To Buy


Specifications


Typical Charpy V-Notch Properties

As welded
Testing Temperature
68 °F

Typical Charpy V-Notch Properties

As welded
Testing Temperature
68 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
MnCuCTiSiNiAlFe
0.4 %0.01 %0.01 %3.1 %0.5 %96 %0.06 %0.04 %

Approvals: VdTÜV; 12659; VdTÜV; 12665
Classifications: SFA/AWS A5.14; ERNi-1; Wire Electrode; EN ISO 18274; S Ni 2061 (NiTi3); Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Nickel (Ni + 2.5 % Ti)