Alloy 4008 has controlled lower levels of impurities than those present in alloys 4010 and 356.0. It is a product that meets the chemistry requirements of AMS 4181. Alloys 356.0, A356.0 and A357.0 are typically used to manufacture sand and permanent mold castings. Alloy 4008 is excellent choice to join or repair these castings, and if needed, it can be heat treated to increased mechanical properties.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 18 % 24 ksi 8 ksi

Typical Weld Metal Analysis %

MnCuZnTiSiMgAlFe
0.01 %0.02 %0.01 %0.1 %7.0 %0.4 %Rem %0.06 %

Approvals: CE, EN 13479, DB, 61.039.10, VdTÜV, 12188
Classifications: EN ISO 18273, S Al Z (AlSi7MgTi), Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.