OK Autrod CuSi Laser


A solid copper wire intended for laser brazing of zinc coated steel sheets. OK Autrod CuSi Laser is especially developed for laser brazing of body-in-white applications within the automotive industry. Compared to a standard CuSi3Mn1 copper wire OK Autrod CuSi Laser provides a more stable brazing process as well as a superior surface finish.

Add to shopping list


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
40 % 51 ksi 19 ksi

Typical Weld Metal Analysis %

MnCuZnSiSnFe
0.9 %96 %0.05 %2.85 %0 %0.05 %

Classifications: SFA/AWS A5.7, ERCuSi-A, Wire Electrode, EN ISO 24373, Cu 6560 (CuSi3Mn1), Wire Electrode