Previous Next

ESAB

OK Autrod 5754


OK Autrod 5754 is a solid aluminium wire with a content of 3 % Mg. It is recommended for welding of Al-Mg alloys with less than 3 % magnesium. The alloy has a relatively high strength and corrosion resistance.

Add to shopping list


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
23 % 33 ksi 16 ksi

Typical Weld Metal Analysis %

MnCuZnTiSiMgAlCrFe
0.26 %0.01 %0.01 %0.13 %0.03 %3.1 %96.19 %0.15 %0.09 %

Approvals: VdTÜV, 04758
Classifications: SFA/AWS A5.10, ER5754, Wire Electrode, EN ISO 18273, S Al 5754 (AlMg3), Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: AlMg