Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
25 % 43 ksi 21 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
18 ft-lb 68 °F

Typical Weld Metal Analysis %

MnCuZnTiSiMgAlCrFe
0.7 %0.01 %0.005 %0.080 %0.05 %5.2 %Rem %0.10 %0.12 %

Approvals: ABS, ER 5556, ClassNK, KA15WCG (I), CWB, A5.10/A5.10M:2012 ER5556
Classifications: SFA/AWS A5.10, ER5556, Wire Electrode, EN ISO 18273, S Al 5556A (AlMg5Mn1Ti), Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: AlMgMn