OK Autrod 5356


OK Autrod 5356 is the most widely used welding alloy and can be classified as a general purpose type filler alloy. OK Autrod 5356 is typically chosen because of its relatively high shear strength. The 5XXX alloy base material, welded with OK Autrod 5356, with a weld pool chemistry greater than 3 % Mg and service temperatures in excess of 65°C are susceptible to stress corrosion cracking. The alloy is non-heat treatable.

Add to shopping list


Specifications


Typical Weld Metal Analysis %

MnCuZnSiMgAlCrFe
0.13 %0.01 %0.01 %0.05 %4.9 %94.560 %0.12 %0.13 %

Approvals: ABS, ER 5356, For lots starting with RB, BV, WB, CE, EN 13479, CWB, A5.10/A5.10M:2012 ER5356, DB, 61.039.01, DNV, 5356, GL, S-AlMg 5, JIS, JIS Z 3232, LR, WB/I1, RINA, WC (*), VdTÜV, 04664
Classifications: JIS Z 3232, A53556, SFA/AWS A5.10, ER5356, Wire Electrode, EN ISO 18273, S Al 5356 (AlMg5Cr(A)), Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: AlMg 5