ESAB

OK Autrod 5183


OK Autrod 5183 was developed to provide the highest strengths possible in the as welded condition of alloy AA 5083 and other similar high magnesium alloys. The more common OK Autrod 5356 will typically fail to meet the as-welded tensile requirements of AA 5083. The alloy is typically utilised in marine and structural applications where high strengths, high fracture toughness for impact resistance and exposure to corrosive elements are important. The alloy is not recommended for elevated temperature applications due to its susceptibility to stress corrosion cracking. The alloy is non-heat treatable.

Add to shopping list


Specifications


Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
66 ft-lb 68 °F

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
66 ft-lb 68 °F

Typical Weld Metal Analysis %

MnCuZnTiSiMgAlCrFe
0.65 %0.01 %0.01 %0.100 %0.04 %4.9 %94.200 %0.08 %0.13 %

Approvals: ABS, ER 5183, For lots starting with RB, BV, WC, CE, EN 13479, ClassNK, KAl5RCG(I-1)(I-4), (only for lots beginning with RB), CWB, A5.10/A5.10M:2012 ER5183, DB, 61.039.03, DNV, 5183, GL, RAlMg4,5Mn, JIS, JIS Z 3232, LR, WC1/I-1, RINA, WC (*), VdTÜV, 04666
Classifications: SFA/AWS A5.10, ER5183, Wire Electrode, EN ISO 18273, S Al 5183 (AlMg4,5Mn0,7(A)), Wire Electrode, JIS Z 3232, A5183, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: AlMgMn