ESAB

OK Autrod 410NiMo


A continuous solid corrosion resisting "410NiMo" type alloyed with 13 % Cr, 4.5 % Ni and 0.5 % Mo. This alloy is used for welding of similar martensitic and martensitic-feritic steels in different applications such as for example hydro-turbines. OK Autrod 410NiMo can be used in combination with OK Flux 10.93.

Where To Buy


Specifications


Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCuCSiNiCr
0.5 %0.6 %0.1 %0.02 %0.4 %4.2 %12.4 %

Classifications: EN ISO 14343-A; S 13 4; Wire Electrode

Alloy Type: Martensitic-ferritic (12 % Cr - 4.5 % Ni - 0.5 % Mo)