Previous Next

ESAB

OK Autrod 1450


OK Autrod 1450 is highly resistant to chemical attack and weathering. The alloy has a small addition of titanium, which has a grain refining effect, which reduces the cracking susceptibility. It has good welding characteristics. A desirable characteristic of the alloy is the bright finishes obtained by anodising. Non-heat treatable.

Add to shopping list


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
35 % 90 MPa 40 MPa

Typical Weld Metal Analysis %

MnCuZnTiSiAlFe
0.02 %0.01 %0.01 %0.12 %0.02 %99.8 %0.16 %

Classifications: EN ISO 18273, S Al 1450 (Al99,5Ti), Wire Electrode