430 Dynagrip Kit

430 Dynagrip Kit

Handy kit containing 4 ft. of 1/16" diameter All-State® No. 430 silver bearing solder and 1/2 fluid oz. of Duzall® flux. Ideal for stainless steel and all metals (except the white metals). Conforms to all pure food laws. Can be used with torch or soldering iron. Working temperature is approximately 430°F (221°C). Tensile strength to 15,000 psi.