OK Autrod 1100


OK Autrod 1100 is highly resistant to chemical attack and weathering. It is a relatively soft alloy that is very formable and is used extensively in thin gauge and foil products. It has good welding characteristics. A desirable characteristic of the alloy is the bright finish obtained by anodising. Non-heat treatable.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
35 % 75 MPa 30 MPa

Typical Weld Metal Analysis %

ELEMENTVALUES
CuBeZnSi+Fe
0.07 %0.0001 %0.01 %0.55 %

Approvals: CWB; AWS A5.10/A5.10M:2012 (ER1100)
Classifications: SFA/AWS A5.10; ER1100; Wire Electrode; EN ISO 18273; S Al 1100 (Al99,0Cu); Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Al