Atom Arc 9018-SR

Atom Arc 9018-SR

Atom Arc 9018SR is an all-position, low hydrogen iron powder electrode with outstanding moisture resistance and welder appeal. The “G” classification of 9018SR is the result of higher Mn and Mo levels and a minimum Ni of 1.1%.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Reduction in Area Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 24 % 68 % 1150 °F 20 hr 99 ksi 87 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Stress Relieved Testing Temp Stress Relieved Testing Time Testing Temperature
Stress Relieved 91 ft-lb 1150 °F 20 hr 60 °F
Stress Relieved 36 ft-lb 1150 °F 20 hr -50 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCuSNiCr
0.016 %1.60 %0.45 %0.01 %0.009 %1.05 %0.03 %

Classifications: ASME SFA 5.5; AWS A5.5; E9018-G H4R