This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

Atom Arc 10018-MM

Atom Arc 10018-MM

Atom Arc 10018-MM electrodes are used to weld low-alloy, high-tensile steels where welds of 100 ksi (690 MPa) minimum tensile strength is required. This electrode is recommended for use in the weld repair and fabrication of Mn-Mo steel castings and armor plate.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Reduction in Area Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 24 % 68 % 1150 °F 1 hr 104 ksi 93 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Stress Relieved Testing Temp Stress Relieved Testing Time Testing Temperature
Stress Relieved 24 ft-lb 1150 °F 1 hr -60 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCSSi
0.018 %1.82 %0.35 %0.09 %0.016 %0.33 %

Classifications: ASME SFA 5.5; AWS A5.5; E10018-D2 H4R