SPOOLARC 83 Tigrod

SPOOLARC 83 Tigrod

Spoolarc 83 contains 0.5% Mo to provide higher deposit strength in both the as welded and stress relieved conditions. It contains high levels of Manganese and Silicon to provide good wetting and good rust and scale tolerance. Spoolarc 83 is also used for all-position welding of high tensile pipe and tubing commonly found in earthmoving and construction equipment.

Where To Buy


Industries

  • Industrial and General Fabrication
  • Automotive
  • Mobile Equipment
  • Ship/Barge Building

Specifications


Typical Weld Metal Analysis %

ELEMENTVALUES
PMnCuMoCSSiNi
0.01 %1.69 %0.17 %0.4 %0.08 %0.011 %0.63 %0.09 %

Approvals: CWB; CSA W48; CSA; CAN/CSA-ISO14341, B-G 55A 3 G4M31 (ER80S-D2); MIL-E-23765/2; 80S-3
Classifications: AWS A5.28; ER80S-D2/ER90S-D2; AWS A5.23; EA3K

Approvals are based on factory location. Please contact ESAB for more information.