Spoolarc 65 Tigrod


Spoolarc 65 is a triple deoxidized (Aluminum, Titanium, Zirconium) welding wire designed for welding over rust and mill scale. The less fluid weld puddle of Spoolarc 65 makes it easy to control when used out of position. Spoolarc 65 is the preferred wire for all position welding of small diameter pipe.

Add to shopping list


Industries

  • Military Applications
  • Pipeline
  • Power Generation
  • Ship/Barge Building

Welding Process

  • Welding-GTAW (TIG - Tungsten Inert Gas )

Specifications


Typical Weld Metal Analysis %

MnMoCAlCrPCuSTiVSiZrNi
1.14 %0.01 %0.06 %0.08 %0.06 %0.004 %0.06 %0.006 %0.10 %0.01 %0.50 %0.04 %0.03 %

Approvals: MIL-E-23765/1, 70S-2, CWB CSA W48, CAN/CSA-ISO14341, B-G 49A 3C G2 (ER49S-2)
Classifications: AWS A5.18, ER70S-2 H4

Approvals are based on factory location. Please contact ESAB for more information.