Typical Tensile Properties

Work Hardening,500 kg. load
Condition Hardness (BHN) Working Temperature Tensile Strength
As Welded 0-200 BHN 1400 to 1750 °F -
500 kg. load
Condition Hardness (BHN) Working Temperature Tensile Strength
As Welded 90-110 BHN - up to 85 ksi