Previous Next

ESAB

All-State 13FC

All-State 13FC

How to order


Specifications


Typical Tensile Properties

Work Hardening,500 kg. load
Condition Hardness (BHN) Working Temperature Tensile Strength
As Welded 0-200 BHN 1400 to 1750 °F -
500 kg. load
Condition Hardness (BHN) Working Temperature Tensile Strength
As Welded 90-110 BHN - up to 85 ksi

View full specs

Brazing alloy designed for wear resistance, overlaying and build-up on ferrous and non-ferrous materials. Deposits easily machined; may remelt again when building up without loss of toughness or overheating of base metal.

Add to shopping list


Specifications


Typical Tensile Properties

Work Hardening,500 kg. load
Condition Hardness (BHN) Working Temperature Tensile Strength
As Welded 0-200 BHN 1400 to 1750 °F -
500 kg. load
Condition Hardness (BHN) Working Temperature Tensile Strength
As Welded 90-110 BHN - up to 85 ksi

x

Inquire about the All-State 13FC



×

Find the Closest Distributor

x

Find the Closest Distributor

x

x

Loading..