All-State 11FC

A high strength brazing alloy for joining ferrous and non-ferrous metals (except white metals), and carbon and alloy steels. Higher strength than ordinary bronze rods, can replace many higher cost silver alloys.

Where To Buy


Specifications


Typical Tensile Properties

500 kg. load
Condition Hardness (BHN) Tensile Strength Working Temperature
As Welded 90-110 BHN up to 85 ksi 1200-1750 °F