All-State GALVOVER

All-State GALVOVER

Use as a substitute for discontinued product All-State #7. Special low temperature alloy used to restore and protect galvanized area of sheet and angle iron. Smooth, with a firm bond that resists corrosion.

Where To Buy


Specifications


Typical Tensile Properties

Condition Working Temperature
As Welded 316 °C