All-State Green Blaster

All-State Green Blaster

A unique chamfering/cutting electrode with 25% more arc blast force. Designed specifically for AC welding machines.~~~Typical Application: Commonly used to remove exisiting cracks or defects prior to wleding with electrodes like All-State Super 4-60 or Super 275.