Previous Next

ESAB

All-State Wear Hard

All-State Wear Hard

Typical Tensile Properties

Heat Treated
Condition Elongation Hardness (HRC) Tensile Strength Yield Strength
As Welded 35-45 % 16 HRC 86-120 ksi 50 ksi
As Welded 36 % 23 HRC 98 ksi 77 ksi