Specifications


Typical Tensile Properties

Heat Treated
Condition Elongation Hardness (HRC) Tensile Strength Yield Strength
As Welded 35-45 % 16 HRC 86-120 ksi 50 ksi
As Welded 36 % 23 HRC 98 ksi 77 ksi

View full specs

High alloy, high strength deposit. For both work-hardening, wear resistant build-up and attachment welding. Use on LaBounty Shear blades to build up cutting edge. Extremely deformation resistant on both carbon and manganese steels.

Add to shopping list


Specifications


Typical Tensile Properties

Heat Treated
Condition Elongation Hardness (HRC) Tensile Strength Yield Strength
As Welded 35-45 % 16 HRC 86-120 ksi 50 ksi
As Welded 36 % 23 HRC 98 ksi 77 ksi