All-State Overlay 4550

Metal-cored, gas-shielded, Argon/CO2 75/25 or Argon Oxygen 98/2 hard-surfacing wire. Tough, shock resistant, tool steel type wire offers good corrosion resistance, excellent metal-to-metal wear and abrasion characteristics. Deposits polish in-service to reduce friction and minimize wear of mating parts. Excellent resistance to heat checking. Multi-layer,crack-free deposits. Deposit hardness 45-50 RC