All-State Overlay 3038

All-State Overlay 3038

A strong,tough, low-alloy, build-up wire for carbon and low alloy steels. Weld deposits are exceptionally sound and dense. Heavy thicknesses are possible without danger of cracking. Machinable with hardness of 33-38 RC.