All-State NI-MATRIX

All-State NI-MATRIX

How to order


Specifications


Typical Tensile Properties

Condition Hardness (BHN) Tensile Strength
As Welded 89 BHN up to 116 ksi

View full specs

All-State Ni-Matrix® has a low hydrogen coating and will deposit austenitic weld metal that is|high in ductility and strength. The welds provide excellent resistance to heavy impact and|compressive loads. The weld metal on the surface will work harden; but below the surface, it will remain tough and ductile. All-State Ni-Matrix® has proven to be superior in performance and less expensive than stainless steel electrodes for most applications on manganese steels. Deposits can be cut with oxygen/fuel torch. Recommended for use where the welds are subject to constant severe impact and heavy compressive tools. Used to attach wear plates, blades, teeth and other parts to heavy equipment. Other applications are mill hammers, crusher liners, dipper teeth and lips, dragline buckets, railroad switches and crusher jaws.

Add to shopping list


Specifications


Typical Tensile Properties

Condition Hardness (BHN) Tensile Strength
As Welded 89 BHN up to 116 ksi

x

Inquire about the All-State NI-MATRIX



×

Find the Closest Distributor

x

Find the Closest Distributor

x

x

Loading..