All-State Kore-Bide 6200

All-State Kore-Bide 6200

Outstanding abrasion resistance on steel or grey cast iron in brick extrusion augers, pump impellers, snow plow shoes, feed screws, dozer end bits, mixer paddles, scraper blades. RC 58 to 62.