Dual Shield 7100SRM

Dual Shield 7100SRM

Dual Shield 7100SRM is an all-position flux cored wire that displays exceptional impact properties in both the as welded and stress relieved condition when used with 75% Ar/25% CO2 shielding. The weld deposit has less than 0.5% nickel which conforms to the A-1 composition in ASME Section IX, QW-440.

Where To Buy


Industries

  • Marine and Offshore
  • Pressure Vessels
  • Ship/Barge Building

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 33 % 1150 °F 8 hr 72 ksi 59 ksi
As Welded 32 % - - 74 ksi 62 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Stress Relieved Testing Temp Stress Relieved Testing Time Testing Temperature
Stress Relieved 63 ft-lb 1150 °F 8 hr -40 °F
Stress Relieved 56 ft-lb 1150 °F 8 hr -50 °F
Stress Relieved 85 ft-lb 1150 °F 8 hr -20 °F
As Welded 69 ft-lb - - -40 °F
As Welded 66 ft-lb - - -50 °F
As Welded 91 ft-lb - - -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnSCSiNi
0.013 %1.40 %0.005 %0.03 %0.41 %0.45 %

Approvals: LR; 5Y40S(H5); CWB; CSA W48: Class E491T-9MJ-H4, E491T-12MJ-H4
Classifications: SFA/AWS A5.36; E71T1-M21-P5-CS2 H4; SFA/AWS A5.36; E71T1-M21-A5-CS2 H4; SFA/AWS A5.20; E71T-9MJH4/T-12MJH4