All-State BRAZALOY 53

All-State BRAZALOY 53

White powder flux for removing oxides of aluminum and zinc based alloys. Active to 700°F. Performs to AWS A5.31, Type FB1-A

Where To Buy


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 28 ksi 371 °C