All-State BRAZALOY 5 Flux

All-State BRAZALOY 5 Flux

Red powder welding flux for cast iron, cast steels, mild and low alloy steels, and stainless steel to cast iron joining. Active from 1400°F to 2000°F. Performs to AWS A5.31