Previous Next

ESAB

All-State Phosphor Bronze C

All-State Phosphor Bronze C

How to order


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 42-50 % up to 65 ksi 37 ksi

View full specs

This bare filler rod produces high strength deposits on phosphor bronze materials. Can be used to join copper and brasses, overlay on cast iron or steel, and join dissimilar metals. Superior for maintenance, repair and fabrication. Use with 100% Argon or 25%/75% Argon/Helium shielding gas mixture.

Add to shopping list


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 42-50 % up to 65 ksi 37 ksi

x

Inquire about the All-State Phosphor Bronze C



×

Find the Closest Distributor