All-State 20

This DC reverse electrode is used for welding aluminum bronze, manganese bronze, silicon bronze, bronze to steel and cast iron, and ferrous alloys. Deposits are strong, dense, ductile, crack free, have good resistance to corrosion, salt water, and many acids and alkalis.

Add to shopping list


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 21-27 % up to 91 ksi 43 ksi