All-State Corecast 8600

All-State Corecast 8600

Continuous flux cored DC reverse composite electrode for joining cast iron to itself or mild steel. Use with 98% Argon/2%Oxygen shielding gas.Machinable.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength
As Welded 12 % 73 ksi