Specifications


Classifications: AWS A5.15

Typical Tensile Properties

Condition Elongation Hardness (BHN) Tensile Strength Yield Strength
As Welded 2-4 % 175-225 BHN up to 50 ksi up to 40 ksi

View full specs

All-position AC/DC reverse electrode for thin sections of cast iron. Provides a high nickel,machinable deposit. For volume welding of defects,filling holes,and salvaging imperfect castings. Good color match. Meets AWS A5.15,Class Eni-Cl-A

Add to shopping list


Specifications


Classifications: AWS A5.15

Typical Tensile Properties

Condition Elongation Hardness (BHN) Tensile Strength Yield Strength
As Welded 2-4 % 175-225 BHN up to 50 ksi up to 40 ksi