Previous Next

ESAB

All-State 4-60T

All-State 4-60T

Top quality most machinable bare rod for TIG welding of thin sections of cast iron up to 3/8". Also joins cast iron to mild steel.

Where To Buy


Specifications


Typical Tensile Properties

Condition Tensile Strength Yield Strength
As Welded up to 80 ksi up to 60 ksi

x
×

Find the Closest Distributor

x

Find the Closest Distributor

x

x

Loading..